Causes and Solutions for Porosity, Shrinkage Cavity and Cracks in Aluminum Die Casting

* : * : admin * : 2026-09-18 14:41:37 * : 17
Causes and Solutions for Porosity, Shrinkage Cavity and Cracks in Aluminum Die Casting
Porosity, shrinkage cavities and cracks are the three most common quality defects in aluminum die casting production. They are the main causes of unqualified air tightness, poor appearance, reduced structural strength and batch scrapping of castings. These defects are generally triggered by improper control of aluminum liquid purity, mold technology, pressure parameters and cooling rhythm. Accurately identifying defect causes and optimizing processes in a targeted manner can effectively improve the qualification rate of die castings, reduce production costs, and ensure product stability and assembly accuracy.
Porosity is mainly caused by residual gas. During smelting, the aluminum liquid absorbs hydrogen and water vapor, while uncleaned impurities and oil stains on furnace materials further introduce gas. Trapped gas cannot be completely discharged during die casting, forming round bubble holes after cooling. Blocked mold exhaust grooves, unreasonable exhaust angles and excessive injection speed will aggravate gas retention. The solutions include thoroughly drying furnace materials, degassing and purifying aluminum liquid, regularly cleaning and optimizing mold exhaust structures, and adopting reasonable injection speed to ensure smooth gas discharge from the cavity.

15041623039542524.JPG


As a solidification shrinkage defect, shrinkage cavities mostly occur at thick-walled positions of castings. Uneven wall thickness, local material accumulation, insufficient holding pressure and short pressure compensation time lead to inadequate liquid replenishment during aluminum liquid solidification, forming irregular concave holes. The improvement measures are optimizing product wall thickness structure to avoid local thick accumulation, increasing holding pressure and duration, and adjusting mold cooling water channels to realize uniform and synchronous solidification and eliminate shrinkage cavities.
Die casting cracks are divided into hot cracks and cold cracks, mostly resulting from stress concentration. Excessively high aluminum liquid temperature, large mold temperature difference and fast ejection speed, together with tiny fillets and abrupt wall thickness changes, generate tensile stress during cooling and shrinkage and eventually cause cracking. In production, strictly control smelting and mold temperature, optimize fillet structures to eliminate sharp corners, reduce ejection speed to release stress evenly during demolding, fundamentally avoid crack defects and stabilize batch production quality.